ABLESTIK FDA 2T

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK FDA2T

Main features

  • 1.20 x 10^14 ohm-cm Volume Resistivity
  • 3-Hour Working Window
  • 1,800 psi Aluminum Lap Shear

Product Description

LOCTITE® ABLESTIK FDA 2T is a two-component, electrically insulating epoxy adhesive developed for medical-device bonding applications. The amber, medium-viscosity system mixes at 100:93 by weight and provides a typical work life of 3 hours. It can be cured for 24 hours at 25°C or accelerated with heat for 1 to 4 hours at 65°C. The cured adhesive has a documented operating-temperature range of -70 to 145°C, a typical volume resistivity of 1.20 × 1014 ohm-cm at 25°C, and aluminum-to-aluminum lap shear strength of 1,800 psi.

Key features

  • Electrically insulating: The cured adhesive has a typical volume resistivity of 1.20 × 1014 ohm-cm at 25°C and dielectric strength of 420 V/mil.
  • Broad operating-temperature range: Documented for operation from -70 to 145°C without implying unchanged properties throughout the range.
  • Room-temperature or heat cure: Guideline schedules include 24 hours at 25°C or 1 to 4 hours at 65°C.

Applications / Suitable for

  • Catheters
  • Hearing aids
  • Dental products
  • Other biomedical instruments and devices
Product Family

ABLESTIK FDA 2T

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry TypeChemistry Type
Epoxy
ColorColor
Amber
Mix RatioMix Ratio
100 : 93
Specific GravitySpecific Gravity
1.12
Work life @25°CWork life @25°C
3 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
70 °C
Operating TemperatureOperating Temperature
-70 to 145 °C
Physical Properties
ViscosityViscosity
26000 mPa.s
Mechanical Properties
ElongationElongation
9 %
Electrical Properties
Volume ResistivityVolume Resistivity
1.20×10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of the mixed adhesive before cure.

Property Value Unit Method / condition
Technology Epoxy — Two-component adhesive system
Color Amber — Mixed adhesive
Mix ratio — resin:hardener 100:93 by weight Resin-to-hardener ratio
Viscosity 26,000 mPa·s (cP) Brookfield RV, spindle 7, 10 rpm at 25°C
Specific gravity 1.12 — Mixed adhesive
Reactive solids content 100 % Typical value
Work life 3 hours Test conditions and endpoint not stated
Cure schedule 24 hours or 1–4 hours — 24 hours at 25°C or 1–4 hours at 65°C; guideline recommendations
Optimal storage 27 °C Store unopened in a dry location; package labeling governs applicable storage information
Technical properties

After-processing / final-state properties

Typical properties and performance data for the cured adhesive. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -70 to 145 °C Documented product range
Coefficient of thermal expansion 5.30 × 10-5 cm/cm/°C Method and temperature region not stated
Glass-transition temperature 70 °C Ultimate Tg; method and cure condition not stated
Hardness 80 Shore D Cure condition not stated
Elongation 9 % Method and cure condition not stated
Volume resistivity at 25°C 1.20 × 1014 ohm-cm Test method and specimen configuration not stated
Dielectric strength 420 V/mil Test method, thickness, and conditioning not stated
Dielectric constant 3.4 — At 25°C and 1 kHz
Dissipation factor 0.02 — At 25°C and 1 kHz
Lap shear strength — aluminum to aluminum 1,800 psi Substrate preparation, bondline, cure condition, test method, and test temperature not stated

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers