BONDERITE M-CR 1500

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-CR 1500

Main features

  • Transparent Chromate Conversion Coating
  • Immersion, Spray, or Brush Application
  • Documented MIL-DTL-81706/MIL-DTL-5541 Qualification

Product Description

BONDERITE® M-CR 1500 AERO is a liquid chromate conversion coating for aluminum and aluminum alloys that produces a protective, colorless conversion coating while preserving the natural appearance of the metal. Designed for immersion, spray, and brush application, it minimizes corrosion, improves paint adhesion, and provides an excellent base for clear organic coatings. The product is listed on the Qualified Products List (QPL) for MIL-DTL-81706 and is approved for applicable methods and classes of MIL-DTL-5541.

Key Features

  • Produces a transparent, colorless chromate conversion coating on aluminum and its alloys.
  • Improves corrosion resistance while enhancing paint adhesion.
  • Suitable for immersion, spray, and brush application.
  • Preserves the characteristic aluminum appearance for clear-finish applications.
  • Listed on the MIL-DTL-81706 Qualified Products List.

Applications / Suitable for

  • Aluminum and aluminum alloys
  • Transparent chromating
  • Paint pretreatment
  • Clear organic coating pretreatment
  • Immersion processing
  • Spray processing
  • Brush application
Product Family

BONDERITE M-CR 1500

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Chromate conversion coating
Thermal Properties
Operating TemperatureOperating Temperature
Ambient °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Product Type Conversion coating — Supplier classification
Physical form Liquid chemical — Supplier description
Application methods Immersion, spray, brush — Supplier recommendation
Qualified specification MIL-DTL-81706 QPL / MIL-DTL-5541 — Supplier published
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Bath make-up 10.5 kg (10 L) per 1,000 L bath — Transparent chromating
Operating temperature 20–40 °C Typical operating range
Operating pH <4.0 — Working bath
Cr(VI) control 6.7–7.7 points Bath control
Immersion time 2–5 minutes Supplier recommendation
Spray time 15–30 seconds Supplier recommendation
Spray pressure 0.5–1.0 bar Spray application
Coating appearance Protective colorless coating — Transparent chromating

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers