BONDERITE S-FN 333

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE S-FN 333

Main features

    Product Description

    BONDERITE® S-FN 333 ACHESON is a resin-bonded dry film lubricant that combines fluorocarbon lubricants with a thermosetting resin to deliver a durable, low-friction coating for demanding industrial applications. Developed for applications beyond conventional fluorocarbon coatings, it provides excellent wear resistance, chemical resistance, and repairability while maintaining low friction and long service life on a wide variety of components. :contentReference[oaicite:0]{index=0}

    Key Features

    • Fluorocarbon-based resin-bonded dry film lubricant for demanding wear applications.
    • Low coefficient of friction combined with excellent durability and wear resistance.
    • Excellent resistance to many acids, bases, solvents, and salt environments.
    • Repairable coating that can be overcoated without removing the original film.
    • Suitable for spray application on a wide range of metal components.

    Applications / Suitable for

    • Business machine parts
    • Valve plugs and valves
    • Drawer guides
    • Window guides
    • Lock assemblies
    • Springs
    • Industrial tools
    • Filter systems
    • Printing equipment
    • Aerospace parts
    • Marine equipment
    • Rails, slides and chutes
    • Closed automotive assemblies
    Product Family

    BONDERITE S-FN 333

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    General Properties
    Product TypeProduct Type
    Resin-bonded fluorocarbon lubricant

    Additional Information

    Technical Properties

    As-Supplied / Before-Processing Properties

    Property Value Unit Method / Condition
    Technology Dry film lubricant — Supplier classification
    Pigment Blend of fluorocarbons — Wet product
    Binder Thermoset — Wet product
    Carrier BONDERITE L-FG SB-3 ACHESON — Wet product
    Diluent BONDERITE L-FG SB-3 ACHESON — Wet product
    Appearance Black liquid — Wet product
    Viscosity 120–150 mPa·s Typical
    Density 1.13 kg/L Typical
    Solids content ~28 % by weight Typical
    Flash point 57 °C Typical
    VOC 808 g/L Typical
    Recommended storage 24°C (75°F) — Original sealed container
    Shelf life 2 years — Original sealed container
    Technical Properties

    After-Processing / Final-State Properties

    Property Value Unit Method / Condition
    Coating color Black — Cured coating
    Coefficient of friction 0.09–0.10 — Static and kinetic
    Recommended dry film thickness 25.4 µm 0.001 in optimum thickness
    Theoretical coverage 6.54 m²/kg @ 25 µm dry film thickness
    Continuous service temperature 204–232 °C 400–450°F
    Salt spray resistance >500 hours Over zinc phosphated surface, 25 µm film
    Hartman Wear Test 200,000 cycles 180 lb load
    Taber Abrasion Test 16.9 mg weight loss 1000 cycles
    Chemical resistance Excellent resistance to selected acids, bases, sodium chloride solutions, ketones and aliphatic solvents — Cured coating
    Typical cure cycle Preheat 149°C for 10 min, then cure at 260°C/15 min, 288°C/9 min, 316°C/5 min, 371°C/1 min, or 399°C/0.5 min — Substrate temperature

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers