COOLTHERM 6756

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM 6756

Main features

  • Adhesion-Promoting Surface Treatment
  • 1 cP Application Viscosity
  • Recommended 3 to 10 um Film Thickness

Product Description

Circalok™ 6756 Primer is a single-component, low-viscosity silicone adhesion promoter developed for electronics applications involving room-temperature-vulcanizing silicone rubbers. The clear or red liquid is applied to prepared metal or glass surfaces before the silicone material to support interfacial adhesion. It has a typical viscosity of 1 cP at 25 °C and a specific gravity of 0.77. Circalok 6756 may be applied by brush or spray, with a recommended primer-film thickness of 3–10 µm, followed by 60–90 minutes of air drying at 25 °C before silicone application.

Key features

  • Silicone adhesion promotion: Supports bonding of RTV silicone rubbers to most metals and glass in electronics applications.
  • Low-viscosity application: Provides a typical viscosity of 1 cP at 25 °C for brush or spray application.
  • Controlled primer layer: Uses a recommended film thickness of 3–10 µm with 60–90 minutes of air drying at 25 °C.

Applications / Suitable for

  • Priming metal surfaces before application of RTV silicone rubber
  • Priming glass surfaces before application of RTV silicone rubber
  • Electronics assemblies requiring silicone-to-substrate adhesion promotion

:contentReference[oaicite:0]{index=0}

Product Family

COOLTHERM 6756

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear or Red Liquid
Specific GravitySpecific Gravity
0.77
Physical Properties
ViscosityViscosity
1 mPa.s
Thermal Properties
Flash PointFlash Point
10 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and application conditions for Circalok 6756 Primer before silicone application. Values are not intended for specification purposes.

Property Value Unit Method / condition
Product form Single-component liquid primer — Silicone adhesion promoter
Appearance Clear or red liquid — As supplied
Dynamic viscosity 1 cP At 25 °C; test method not stated
Specific gravity 0.77 — Test temperature and method not stated
Recommended primer-film thickness 3–10 µm Applied by brush or spray for optimum adhesion
Air-drying time 60–90 minutes At 25 °C before applying RTV silicone

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers