DOWSIL PR1200

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

DOWSIL PR1200

Main features

  • Adhesion-Promoting Surface Treatment
  • Wipe, Spray, or Dip Application
  • 1 to 2-Hour Cure Window

Product Description

DOWSIL™ PR-1200 RTV Prime Coat is a one-part, naphtha-based liquid adhesion primer for improving the bond of moisture-cure RTV and heat-cure silicone elastomers to difficult substrates. Supplied in clear and red variants, it can be used on many metals, aluminum, glass, ceramics, masonry, granite, FR-4, and selected plastics. The primer is applied as a very light, even film by wiping, dipping, or spraying, then moisture-cured at room temperature before silicone application. The thin reactive layer supports silicone adhesion without becoming a bulk coating. Variant-specific typical data include 4.9% nonvolatile content for clear and 4.5% for red, with an 18-month shelf life from manufacture.

Key features

  • Broad substrate range: Supports priming on many metals, aluminum, glass, ceramics, masonry, granite, FR-4, and selected plastics.
  • Thin-film application: Apply a very light, even coat by wiping, dipping, or spraying; remove excess material to avoid over-application.
  • Controlled room-temperature cure: Generally cures for 1–2 hours at room temperature and 20–90% relative humidity before silicone application.
  • Clear and red variants: Two color options are available with variant-specific nonvolatile-content data.
  • Documented aluminum peel result: Both variants report a typical 180-degree peel strength of 37 ppi on aluminum.

Applications / Suitable for

  • RTV and heat-cure silicone adhesion to metals, aluminum, glass, and ceramics
  • Silicone priming on masonry, granite, and plywood
  • Silicone adhesion to FR-4 and selected structural plastics
  • Surface preparation for silicone sealants, coatings, and elastomers

Technical Specifications

No specifications available.

Additional Information

Surface Treatments | Adhesion Primers & Promoters

DOWSIL™ PR-1200 RTV Prime Coat

DOWSIL™ PR-1200 RTV Prime Coat is a one-part, naphtha-based surface treatment used to enhance adhesion of moisture-cure RTV and heat-cure silicones to metals, glass, ceramics, masonry, FR-4, and selected plastics. Clear and red variants use the same thin-coat application and room-temperature moisture-cure process.

One-part liquid primer Naphtha-based carrier Clear and red variants Wipe, dip or spray application 1–2 hour room-temperature cure

As supplied

Typical As-Supplied Properties

Typical values are not intended for use in preparing specifications. Variant-specific values are identified where applicable.

Property Value Unit Method / condition
Product form One-part liquid primer — As supplied
Carrier solvent Naphtha — Current supplier product literature
Available colors Clear and red — Commercial variants
Nonvolatile content - clear 4.9 % Typical value
Nonvolatile content - red 4.5 % Typical value
Flash point, closed cup 13 (55) °C (°F) Dow Corporate Test Method 0917, based on ASTM D3278
Volatile organic content 748 g/L Typical value
Shelf life 18 months From date of manufacture; use the product label's Use Before date
Processing

Surface Preparation and Primer Application

PR-1200 should form a very thin, uniform treatment on a clean, dry substrate. Control surface preparation, application quantity, ambient cure conditions, and the interval before applying the silicone.

Surface preparation: Remove oils and contaminants with a suitable solvent. Light abrasion is recommended when practical, and a final acetone or IPA wipe may be helpful. Allow cleaning solvents to evaporate completely.
Primer application: Apply a very light, even coat by wiping, dipping, or spraying. Wipe off excess material. For dip or spray use, dilution by a factor of 2 to 4 with additional solvent may reduce excessive build-up.
Cure conditions: Cure generally occurs at room temperature for 1 to 2 hours at 20 to 90% relative humidity. Lower temperature or humidity requires more time; temperatures above 60°C (140°F) are not recommended.
Storage and Handling

Store below 32°C (90°F), keep containers tightly closed, minimize headspace, and protect the primer from moisture. Pour only a small working quantity into a clean, dry container and discard unused working material. Do not use material that becomes milky or develops a large amount of white precipitate. Use the labeled Use Before date.

Application Controls

Prevent over-application
Use only enough primer to lightly wet the surface. A white, chalky or powdery film indicates excessive build-up, which can reduce adhesion. Clean an over-primed surface and apply a new thin coat.
Keep working material fresh
Limit the amount exposed to ambient moisture, recap the original container promptly, and refresh primer on the application cloth every 3 to 5 minutes. After cure, apply the silicone within the validated process window; if a long delay occurs, re-cleaning and re-priming may be required.

Clear and Red Variant Comparison

The two PR-1200 variants share the same primer function and application approach. Use the variant-specific typical data below when selecting and documenting the commercial form.

Variant Nonvolatile content 180-degree peel strength on aluminum Selection note
Clear 4.9% 37 ppi Clear commercial variant; 18-month shelf life from manufacture.
Red 4.5% 37 ppi Red commercial variant; 18-month shelf life from manufacture.

Values are typical and not specification limits. Current product literature recommends storage below 32°C (90°F); follow the labeled Use Before date and regional product documentation.

Applications

Supported Application Contexts

PR-1200 is used as a thin surface treatment before applying RTV or heat-cure silicone materials. The substrate and silicone system should be evaluated together under the intended preparation, cure, and service conditions.

Silicone bonding interface on metal, glass, and ceramic substrates
Metals, Glass and Ceramics
Use PR-1200 to promote adhesion of RTV and heat-cure silicones to many metals, including aluminum, as well as glass and ceramic surfaces. Surface cleaning and complete solvent evaporation remain essential before priming.
Silicone sealing interface on masonry, granite, and plywood
Masonry, Granite and Plywood
The primer may be used to prepare construction-related surfaces such as masonry, granite, and plywood before silicone sealant or coating application. Porosity, surface condition, and primer uptake should be validated for the specific material.
Silicone adhesion evaluation on FR-4 and structural plastic substrates
FR-4 and Selected Plastics
PR-1200 supports evaluation of silicone adhesion to FR-4 and selected structural plastics. Because plastics vary in composition and surface energy, confirm cleaning, wetting, cure compatibility, and final adhesion on the exact grade.
Product resource

Primer Selection and Application Guide

DOWSIL™ Primers, Prime Coats, and Adhesion Promoters
This supplier brochure provides portfolio-level guidance on surface preparation, thin-film application, cure conditions, storage, and primer selection. It includes DOWSIL™ PR-1200 in the selection guide and summarizes recommended priming steps for process planning.
Next steps

PR-1200 Primer Evaluation and Support

Contact Krayden to review substrate type, silicone chemistry, surface preparation, application method, cure conditions, and clear-versus-red variant needs for DOWSIL™ PR-1200 RTV Prime Coat. Krayden can support product selection, sample requests, technical-data review, and planning for controlled primer evaluation in your assembly or sealing process.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers