EPOCAST 1648

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1648

Main features

  • Low-Density Flame-Retardant Syntactic
  • Controlled Syntactic Dispensing
  • BMS 5-28 Type 18 Class 1

Product Description

EPOCAST® 1648 A/B is a two-component, low-density, flame-retardant syntactic epoxy adhesive for aerospace honeycomb and structural filling applications. The mixed material is a non-flowing paste with a typical density of 0.65–0.70 g/cm³, an 18-minute gel time at 25°C, and sufficient extrudability for dispensing through a 3 mm nozzle. It can be applied using meter-mix equipment, Semco™ cartridges, or hand mixing. After cure, the system provides compressive, lap-shear, insert pull-out, and torque performance for demanding lightweight assemblies. It is qualified to BMS 5-28, Type 18, Class 1.

Key features

  • Low-density, non-flowing formulation: The mixed adhesive has a typical density of 0.65–0.70 g/cm³ and remains in place after application.
  • Dispensing flexibility: Suitable for meter-mix equipment, Semco™ cartridges, or hand mixing and extrusion through a 3 mm nozzle.
  • Aerospace flame-performance qualification: Qualified to BMS 5-28, Type 18, Class 1, with a reported FAR 25.853 self-extinguishing time below five seconds.

Applications / Suitable for

  • Aerospace fastener potting
  • Edge filling and sealing
  • Tab-and-slot joining
  • Honeycomb core reinforcement
Product Family

EPOCAST 1648

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White
Density (g)Density (g)
0.68 g/cm3
Mix RatioMix Ratio
100:20

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material, dispensing, and cure data. Values are typical and are not product specifications.

Property Value Unit Method / condition
Appearance Part A: off-white paste; Part B: amber paste; mixed: off-white paste — Visual
Consistency Part A: paste; Part B: soft paste; mixed: paste — ASTM D2196 at 25°C
Density Part A: 0.59–0.64; Part B: 1.05–1.15; mixed: 0.65–0.70 g/cm³ ASTM D1875
Mix ratio, A:B 100:20 Parts by weight Recommended ratio
Gel time 18 min ASTM D2471; 60 g at 25°C
Extrusion rate 180–220 g/min OEM method; measured at 10 minutes
Slump ≤0.3 in (≤7.6 mm) ASTM D2202
Typical cure cycles 3 days at 25°C, or gel at 25°C followed by at least 5 hours at 52°C — Typical cure schedules
Technical properties

After-processing / final-state properties

Typical cured-material properties. Hot/wet exposure consisted of seven days at 25°C followed by 14 days at 71°C and 95% relative humidity. Values are typical and are not product specifications.

Property Value Unit Method / condition
Cured density 0.68 ± 0.02 g/cm³ (42.5 ± 1.2 lb/ft³) ASTM D1622
Compressive strength Standard: 7,250 ± 750; hot/wet: 6,750 ± 80 psi (50 ± 5.2; 46.5 ± 0.6 MPa) ASTM D695 at 23°C
Compressive modulus Standard: 350 ± 50; hot/wet: 290 ± 10 ksi (2.4 ± 0.3; 2.0 ± 0.1 GPa) ASTM D695 at 23°C
Tensile lap-shear strength Standard: 2,050 ± 150; hot/wet: 1,900 ± 60 psi (14.1 ± 1.0; 13.1 ± 0.4 MPa) ASTM D1002; aluminum-to-aluminum at 23°C
Insert pull-out strength 400 ± 50 lb (1.8 ± 0.2 kN) OEM method
Insert torque strength 120 ± 20 in·lb (13.6 ± 2.3 N·m) OEM method
Self-extinguishing time <5 s FAR 25.853; 12-second vertical test
Smoke density 160 — FAR 25 Appendix F V(b); measured at four minutes

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers