EPOCAST 35-A/927

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 35-A/927

Main features

  • 149 deg C Laminating Performance
  • 4 to 5-Hour Work Life
  • BMS 8-214 Glass-Fabric Lamination

Product Description

EPOCAST® 35 A / Hardener 927 is a two-component, solvent-free epoxy laminating system for repairing and fabricating laminated composite structures. The 100:25 weight-ratio system has a medium mixed viscosity that readily wets glass fabrics and provides a typical 4–5 hour work life at 25°C for extended fabrication and large repair procedures. The cured system is designed to perform at temperatures up to 149°C and can be processed using either of two elevated-temperature cure cycles. EPOCAST 35 A / Hardener 927 is qualified to BMS 8-214.

Key features

  • High-temperature performance: Designed to perform at temperatures up to 149°C after the specified elevated-temperature cure.
  • Extended working time: Provides a typical 4–5 hour work life for large composite repairs and extended fabrication procedures.
  • Glass-fabric wetting: The 7,000 cP mixed system readily wets glass fabrics for laminated composite construction and repair.

Applications / Suitable for

  • Repair of laminated composite structures
  • Fabrication of glass-fabric composite laminates
  • Composite applications requiring elevated-temperature performance
Product Family

EPOCAST 35-A/927

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Amber
Density (g)Density (g)
1.13 g/cm3
Mix RatioMix Ratio
100:25
Physical Properties
ViscosityViscosity
7000 mPa.s
Viscosity (Part A)Viscosity (Part A)
3200 mPa.s
Viscosity (Part B)Viscosity (Part B)
25000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the individual components and mixed system. These values are not product specifications.

Property Value Unit Method / condition
Appearance Amber / dark amber / amber — Visual; resin / hardener / mixed system
Density at 25°C 1.19 / 1.00 / 1.13 g/cm³ ASTM D792; resin / hardener / mixed system
Viscosity at 25°C 3,200 / 25,000 / 7,000 cP ASTM D2196; resin / hardener / mixed system
Mix ratio 100:25 Parts by weight EPOCAST 35 A Resin : Hardener 927
Work life 4–5 Hours 100 g mixed mass at 25°C
Typical cure cycles 4 at 83°C or 2 at 121°C Hours Cure 1 or Cure 2
Storage temperature 2–8 °C Dry place in original sealed containers
Shelf life 1 Year From shipment under stated storage conditions
Technical properties

After-processing / final-state properties

Typical cured properties are shown as Cure 1 / Cure 2. Cure 1 is 4 hours at 83°C; Cure 2 is 2 hours at 121°C.

Property Value Unit Method / condition
Durometer hardness 93 / 93 Shore D ASTM D2240; Cure 1 / Cure 2
Flexural strength 77.4 (534) / 104.0 (717) ksi (MPa) ASTM D790; as cured at 25°C; Cure 1 / Cure 2
Flexural strength after boiling-water exposure 52.1 (359) / 68.6 (473) ksi (MPa) ASTM D790; after 2 hours boiling water, tested at 25°C
Flexural modulus 3,021 (20,827) / 3,801 (26,206) ksi (MPa) ASTM D790; as cured at 25°C; Cure 1 / Cure 2
Compressive strength 61.4 (423) / 71.9 (496) ksi (MPa) ASTM D695; as cured at 25°C; Cure 1 / Cure 2
Compressive strength at 149°C 2.0 (13.8) / 3.4 (23.4) ksi (MPa) ASTM D695; tested at 149°C; Cure 1 / Cure 2
Compressive modulus 3,751 (25,862) / 4,031 (27,793) ksi (MPa) ASTM D695; as cured at 25°C; Cure 1 / Cure 2
Tensile lap shear — / 1,090 (7.5) psi (MPa) ASTM D1002; aluminum-to-aluminum, as cured at 25°C; Cure 2 value only

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers