BGT-PO180 | Polyolefin Back Grinding Tape

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

BGT-PO180 | Polyolefine Back Grinding Tape

Main features

  • 180 µm film thickness
  • Urethane UV removable adhesive
  • High accuracy and easy to peel

Product Description

LINQTAPE™ BGT-PO180 is a translucent polyolefin (PO) tape used in the wafer back grinding process. It is compatible to the BG standard, and is highly accurate. The tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties. PO tapes have the same strong adhesion as a PET tape but are more easily removed from the substrate. This makes it ideal for applications where easy removal without any residue left behind is required. BGT-PO180 is has a low-viscosity adhesive, and is resistant to warpage. 

LINQTAPE™ BGT-PO180 can be peeled by using UV. To ensure a clean substrate after removing the tape, BGT-PO180 utilizes a technology through which after applying UV light, the adhesive (18,000 N/25mm) becomes less tacky (80 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass and other sensitive substrates. BGT-PO180 is a 150µm PO film, with a one-sided 30µm urethane adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Back grinding standard compatible
  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Back grinding 
  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

LINQ BGT-PO180

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Acrylic
AppearanceAppearance
Transparent
Film ThicknessFilm Thickness
150 µm
Release LinerRelease Liner
PET
Total ThicknessTotal Thickness
180 μm
Mechanical Properties
Adhesion StrengthAdhesion Strength
64748 Oz/in
ElongationElongation
830 lengthwise, 740 crosswise %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
34 lengthwise, 30 crosswise N/cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers