PIT1A-ESD | 1mil Antistatic ESD Polyimide (Kapton) Tape with Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

1mil Antistatic ESD Polyimide X-Section1mil Antistatic ESD Polyimide Tape with Acrylic Adhesive

Main features

  • 1 mil polyimide film
  • Acrylic adhesive
  • >6000V breakdown voltage

Product Description

LINQTAPE™ PIT1A-ESD Series is a high-temperature resistant, antistatic-treated polyimide film mounted with an acrylic adhesive. It is designed for both masking and temporary bonding in many high-temperature applications in semiconductor, electronic, automotive, and other general manufacturing industries.

LINQTAPE™ PIT1A-ESD Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 155°C (311°F).

LINQTAPE™ PIT1A-ESD Series comes as a standard in 36-yard (33m) lengths of varying widths, but longer rolls may be available upon request. Please note that batches after April 2024 will all come with a release liner.

 

Key Features:

  • Antistatic coating to dissipate electrostatic charge
  • Pressure-sensitive acrylic adhesive
  • Excellent insulating properties

 

Product Family

LINQ PIT1A-ESD

1. Select Width
2. Select Length
Price starting from €9.62
Product availability
EU Shipping in 2 weeks
Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Acrylic
Adhesive ThicknessAdhesive Thickness
38.1 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Amber
Film ThicknessFilm Thickness
25.4 µm
Release LinerRelease Liner
Yes
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single-Sided
Special LayerSpecial Layer
Antistatic Polymer Coating
Total ThicknessTotal Thickness
63.5 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
155 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
6000 V
Dielectric StrengthDielectric Strength
237 kV/mm
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
25 Oz/in
ElongationElongation
70 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
53 N/cm

Additional Information

Application Ideas

  • Dissipate electrostatic charges
  • Protection of static-sensitive devices
  • Temporary bonding of thermocouples for oven profiling
  • Bonding of devices before solder reflow
  • Splicing of insulation layers

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers