PIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

Die Cut Kapton Tape on Release LinerPIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release LinerPIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release LinerPIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release LinerPIT2S-RL | 2-mil Polyimide (Kapton) Tape with Silicone Adhesive on Release Liner2-mil Polyimide (Kapton) Tape Silicone Adhesive Release Liner2mil Polyimide High Temperature Dicing Tape | Release Liner Structure

Main features

  • 2 mil polyimide film
  • Silicone adhesive
  • >11000V breakdown voltage

Product Description

LINQTAPE™ PIT2S-RL-Series s is a high-temperature resistant polyimide tape on a 2 mil PET release liner. It is designed primarily for high temperature temporary bonding applications and it removes cleanly without adhesive residue after exposure to heat or chemicals. It may also be used in electrical insulation applications that require Class H tape grade.

LINQTAPE™ PIT2S-RL-Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 260°C (500°F).

LINQTAPE™ PIT2S-RL-Series comes as a standard in 36 yard (33m) lengths of varying widths, but longer rolls may be available upon request.

Product Family

LINQ PIT2S-RL

1. Select Width
2. Select Length
Price starting from €6.87
Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Silicone
Adhesive ThicknessAdhesive Thickness
38.1 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Amber
Film ThicknessFilm Thickness
50.8 µm
Release LinerRelease Liner
Single Release Liner
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single-Sided
Special LayerSpecial Layer
None
Total ThicknessTotal Thickness
88.9 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
260 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
>11000 V
Dielectric StrengthDielectric Strength
197 kV/mm
Volume ResistivityVolume Resistivity
10000000000000 Ohms⋅cm
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
26 Oz/in

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers