LOCTITE EA E-120HP

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA E-120HP

Main features

  • 120-Minute Working Life
  • Peel, Impact, Thermal-Shock, and Chemical Resistance
  • Aerospace and Industrial Bonding

Product Description

LOCTITE® EA E-120HP is a two-component, high-viscosity epoxy adhesive with an extended working life and room-temperature cure. The resin and polyamide hardener mix at a 2:1 ratio by volume to form a tough, amber-beige bondline with resistance to peel, impact, thermal shock, solvents, and chemicals. The adhesive bonds dissimilar materials, including aluminum, steel, other metals, plastics, and ceramics. Its combination of a 120-minute working life and durable cured properties supports aerospace nose-cone bonding and low-stress general industrial assemblies requiring high peel and impact strength.

Key features

  • Extended working life: The mixed adhesive has a typical working life of 120 minutes for applications requiring additional assembly time.
  • Tough cured bondline: The room-temperature-curing epoxy is formulated for resistance to peel, impact, and thermal shock.
  • Broad substrate bonding: Suitable for bonding aluminum, steel, other metals, plastics, and ceramics.

Applications / Suitable for

  • Aerospace nose-cone bonding
  • Low-stress general industrial assemblies requiring high peel and impact strength
  • Bonding dissimilar metals, plastics, and ceramics
Product Family

LOCTITE EA E-120HP

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.1
Physical Properties
Tack-Free TimeTack-Free Time
140 minutes
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
90 °C
Mechanical Properties
ElongationElongation
10 %
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed adhesive.

Property Value Unit Method / condition
Appearance Resin: off-white to beige liquid; hardener: amber liquid; mixture: amber-beige — Visual
Mix ratio, resin:hardener 2:1 By volume Two-component system
Mix ratio, resin:hardener 100:46 By weight Two-component system
Resin viscosity 41,000–61,000 mPa·s (cP) Brookfield RVT, 25 °C, spindle 7, 50 rpm
Hardener viscosity 2,000–4,000 mPa·s (cP) Brookfield RVT, 25 °C, spindle 5, 50 rpm
Specific gravity Resin: 1.1; hardener: 1.0; mixed: 1.1 — At 25 °C
Working life 120 min Mixed adhesive
Tack-free time 140 min Mixed adhesive; low humidity

After-processing / final-state properties

Typical physical, electrical, and adhesive properties after the specified cure conditions.

Property Value Unit Method / condition
Glass transition temperature 90 °C ASTM E1640; cured 7 days at 22 °C
Shore hardness 76–90 Durometer D ISO 868; cured 16–18 h at 22 °C followed by 2 h at 65 °C
Elongation 10 % ISO 527-2; cured 7 days at 22 °C
Tensile strength 41 N/mm² ISO 527-3; cured 7 days at 22 °C
Dielectric breakdown strength 25 kV/mm IEC 60243-1; cured 7 days at 22 °C
Lap shear strength, aluminum ≥13.7 N/mm² Acid-etched aluminum; cured 2 h at 65 °C
Lap shear strength, steel 30 N/mm² Grit-blasted steel; cured 12 h at 65 °C
Lap shear strength, aluminum 33 N/mm² Acid-etched and abraded aluminum; 0.1–0.2 mm gap; cured 12 h at 65 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers