LORD 7545A/B

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7545A/B

Main features

  • Non-Sag Urethane Bonding
  • 3 to 5-Minute Working Window
  • 30-Minute Handling Time

Product Description

LORD® 7545-A/B Urethane Adhesive is an equal-mix, two-component structural urethane adhesive system for bonding fiberglass-reinforced plastic (FRP), sheet molding compound (SMC), other plastics, primed metals and supported dissimilar substrates. The 100% solids system has non-sag paste rheology for bead placement on vertical and overhead joints. When paired with LORD® 7545-B curative, it provides a 3–5 minute working time and reaches handling strength in approximately 30 minutes at 75°F (24°C).

Key Features

  • Equal-volume mixing at a 1:1 resin-to-curative ratio for cartridge or meter/mix/dispense processing.
  • Fast A/B processing window with a 3–5 minute working time and approximately 30-minute handling time at 75°F (24°C).
  • Non-sag, environmentally resistant system that maintains bead placement and resists weathering, humidity, salt spray and solvents after cure.

Applications / Suitable for

  • FRP and SMC structural bonding
  • Plastic-to-plastic assemblies
  • Composite or plastic bonding to primed metals
  • Vertical, overhead and supported mixed-material joints
Product Family

LORD 7545A/B

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
A (Resin)/ B(Curative): Brown/Black Paste
DensityDensity
A (Resin): 1498 -1534 | B(Curative): 1294 -1342 kg/m3
Physical Properties
ViscosityViscosity
A (Resin): 25,000 - 70,000 | B (Curative): 230,000 - 650,000 mPa.s
Thermal Properties
Flash PointFlash Point
A (Resin)/ B(Curative): >93 °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 7545-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property 7545-A Resin 7545-B Curative Mixed System Method / Condition
Appearance Brown paste Off-white or black paste — Typical
Viscosity 25,000–70,000 cP 230,000–650,000 cP — Brookfield at 77°F (25°C)
Density 12.5–12.8 lb/gal
(1498–1534 kg/m³)
10.8–11.2 lb/gal
(1294–1342 kg/m³)
— Typical
Flash Point >200°F
(>93°C)
>200°F
(>93°C)
— Closed cup
Mix Ratio 1 part 1 part by volume
0.87 part by weight
1:1 by volume
1:0.87 by weight
Resin to curative
Solids Content by Weight — — 100% Mixed adhesive system
Working Time — — 3–5 minutes At 75°F (24°C); LORD® 7545-A/B configuration
Time to Handling Strength — — 30 minutes At 75°F (24°C); LORD® 7545-A/B configuration
Recommended Bondline Thickness — — 10–40 mil
(254–1016 µm)
For optimum adhesion
Shelf Life 6 months 6 months — Store unopened at or below 77°F (25°C)
Technical Properties

As-Supplied / Before-Processing Properties

Typical component and mixed-system properties for LORD® 7545-A/B Urethane Adhesive. Values are typical and are not intended for specification purposes.

Property 7545-A Resin 7545-B Curative Mixed System Method / Condition
Appearance Brown paste Off-white or black paste — Typical
Viscosity 25,000–70,000 cP 230,000–650,000 cP — Brookfield at 77°F (25°C)
Density 12.5–12.8 lb/gal
(1498–1534 kg/m³)
10.8–11.2 lb/gal
(1294–1342 kg/m³)
— Typical
Flash Point >200°F
(>93°C)
>200°F
(>93°C)
— Closed cup
Mix Ratio 1 part 1 part by volume
0.87 part by weight
1:1 by volume
1:0.87 by weight
Resin to curative
Solids Content by Weight — — 100% Mixed adhesive system
Working Time — — 3–5 minutes At 75°F (24°C); LORD® 7545-A/B configuration
Time to Handling Strength — — 30 minutes At 75°F (24°C); LORD® 7545-A/B configuration
Recommended Bondline Thickness — — 10–40 mil
(254–1016 µm)
For optimum adhesion
Shelf Life 6 months 6 months — Store unopened at or below 77°F (25°C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers