PERMABOND 108

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 108

Main features

  • 400 to 600 mPa s Viscosity Range
  • 10-Second Fixturing Time
  • 25 kV/mm Dielectric Strength

Product Description

PERMABOND® 108 Cyanoacrylate Adhesive is a single-component, intermediate-viscosity ethyl cyanoacrylate adhesive for bonding through small to intermediate gaps. Its 400–600 mPa·s viscosity supports controlled application and automated dispensing while retaining fast fixture performance. Typical handling strength is reached in approximately 10 seconds on steel, Buna N rubber, and phenolic, with full strength developing in 24 hours. The adhesive bonds plastics, rubber, and metals and provides a maximum recommended gap fill of 0.25 mm. After cure, it delivers high shear strength on steel and selected plastics, 85 Shore D hardness, and useful electrical insulation properties for industrial assembly.

Key features

  • Intermediate viscosity: A viscosity of 400–600 mPa·s supports controlled dispensing and bonding across gaps up to 0.25 mm.
  • Fast fixture performance: Typical handling strength is reached in approximately 10 seconds on steel, Buna N rubber, and phenolic.
  • Multi-material bonding: Documented performance covers steel, ABS, PVC, and polycarbonate, with general suitability for plastics, rubber, and metals.

Applications / Suitable for

  • Automated adhesive dispensing
  • Bonding parts with small to intermediate gaps
  • High-speed industrial assembly
  • Bonding plastics, rubber, and metals
Product Family

PERMABOND 108

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Liquid
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
ColorColor
Colourless
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
400-600 mPa.s
Mechanical Properties
Impact StrengthImpact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm
Maximum gap fillMaximum gap fill
0.25 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 400–600 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.25 mm Equivalent source value 0.008 in
Fixture time — steel 10 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 10 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

After-processing / final-state properties

Typical cured performance values. Bond strength varies with substrate, surface preparation, joint gap, and cure conditions.

Property Value Unit Method / condition
Shear strength — steel 20–22 N/mm² ISO 4587; equivalent source range 2,900–3,200 psi
Shear strength — ABS 8 N/mm² ISO 4587; substrate failure reported
Shear strength — PVC >10 N/mm² ISO 4587; substrate failure reported
Shear strength — polycarbonate 10 N/mm² ISO 4587; substrate failure reported
Impact strength 3–5 kJ/m² ASTM D950
Hardness 85 Shore D ISO 868
Dielectric strength 25 kV/mm Typical cured electrical property
Dielectric constant 2.5 — At 10 kHz

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers