PERMABOND 2010

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 2010

Main features

  • Thixotropic Vertical-Surface Control
  • Up to 0.5 mm Gap Filling
  • 25 kV/mm Dielectric Strength

Product Description

PERMABOND® 2010 Cyanoacrylate Adhesive is a thixotropic, fast-setting, single-component ethyl cyanoacrylate adhesive designed for vertical, porous, and gap-filling applications. Its semi-gel consistency helps resist running and supports controlled dispensing on metals, plastics, elastomers, ceramics, and wood. At 25 °C, the adhesive provides a viscosity of 2,000–2,500 mPa·s at 20 rpm and 10,000–20,000 mPa·s at 2 rpm, reflecting its thixotropic behavior. It fills gaps up to 0.5 mm and typically reaches handling strength in 10–15 seconds on steel, Buna N rubber, and phenolic, with full strength developing in 24 hours.

Key features

  • Thixotropic semi-gel consistency: Helps prevent running on vertical surfaces while supporting accurate dispensing and placement.
  • Maximum gap-filling capability: Suitable for joints with gaps up to 0.5 mm.
  • Fast fixture performance: Typical handling strength is achieved in 10–15 seconds on steel, Buna N rubber, and phenolic.

Applications / Suitable for

  • Vertical bonding applications
  • Porous substrates
  • Gap-filling joints up to 0.5 mm
  • Bonding metals, plastics, elastomers, ceramics, and wood
  • High-speed industrial assembly
Product Family

PERMABOND 2010

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Liquid
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
ColorColor
Colourless
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
2,000-2,500 mPa.s mPa.s
Mechanical Properties
Impact StrengthImpact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
25 kV/mm
Maximum gap fillMaximum gap fill
0.5 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless semi-gel — Thixotropic consistency
Viscosity 2,000–2,500 mPa·s At 25 °C and 20 rpm
Viscosity 10,000–20,000 mPa·s At 25 °C and 2 rpm
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.5 mm Equivalent source value 0.02 in
Fixture time — steel 10–15 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 10–15 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

After-processing / final-state properties

Typical cured performance values. Bond strength varies with substrate, surface preparation, joint gap, and curing conditions.

Property Value Unit Method / condition
Shear strength — steel 19–23 N/mm² ISO 4587; equivalent source range 2,800–3,300 psi
Shear strength — aluminum 7–9 N/mm² ISO 4587; equivalent source range 1,000–1,300 psi
Shear strength — zinc 10 N/mm² ISO 4587; equivalent source value 1,500 psi
Shear strength — phenolic 14 N/mm² ISO 4587; equivalent source value 2,000 psi
Impact strength 3–5 kJ/m² ASTM D950
Hardness 85 Shore D ISO 868
Dielectric strength 25 kV/mm Typical cured electrical property
Thermal conductivity 0.1 W/(m·K) Typical cured thermal property

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers